D3 (W.Nr. 1.2080), X210Cr12 | Chemical composition (%) | C | Mn | Si | P | S | Cr | 1.90-2.20 | 0.20-0.60 | 0.10-0.60 | max. 0.030 | max. 0.030 | 11.00-13.00 | | | | | | | | | | >> Standard | EN ISO 4957 | | | | | | | | | | | | | Steel characteristics: | Chrome steel of ledeburitic type for cold work. Recognized for high resistance against wear, high compression strength,and low deformation durning heat processing. | Application: | Devices for cutting, pressing and perforation of sheet metal up to approx.3 mm thickness casting moulds for deep traction, devices for cold cutting. | Delivery condition: | Soft annealed steel, max.248 HB. | Physical features: | Temperature [oC] | 20-100 | 20-200 | 20-300 | 20-400 | Thermal expansion | 10,8 | 11,6 | 12,3 | 12,5 | Temperature [oC] | 20 | 350 | 700 | | Heat conductivity | 16,7 | 20,5 | 24,1 | | | | | | | | | | | >> Recommended temperatures for heat processing | | | | | | | | | | Soft annealing: | Temperature [oC] | Cooling | | 800-840 | Furnace | | Annealing after decreasing stress: | Temperature [oC] | Cooling | | 600-650 | Furnace | | Hardening and tempering: | Austenization [oC] | Hardening | | 930-980 | Oil, pressure gas(N2) air, warm bath | | | |
|
|
Last Updated ( Salı, 30 Aralık 2008 )
|