>>H11 (W.Nr. 1.2343), X37CrMoV5-1 (mod.S10) | Chemical composition (%) | C | Mn | Si | P | S | Cr | Mo | V | 0.33-0.41 | 0.25-0.50 | 0.80-1.20 | max. 0.03 | max. 0.01 | 4.8-5.5 | 1.1-1.5 | 0.3-0.5 | | | | | | | | | | | | >> Standard | EN ISO 4957 | | | | | | | | | | | | | | | | | Steel characteristics: | Medium alloyed tool steel for cold work, great robustness and heat resistance, high strength in hot environments, high robustness inhot environments and low dimensional during heat processing. Steel has for use due to decreased sulphur level. | Application: | Devices for forming and cutting of metals under heat. Casts for pessure casting of non-ferrous metals. | Delivery condition: | Soft annealed steel, max.229 HB. For more demanding use, it is prefered to use EFS steel with guaranteed structure and sulphur content=max.0,005% | Physical features: | Temperature [oC] | 20-100 | 20-250 | 20-500 | | | Thermal expansion [10-6.K-1] | 10,5 | 11,3 | 12,1 | | | Temperature [oC] | 20 | 350 | 700 | | | Heat conductivity [W.m-1.K-1] | 23 | 25 | 27 | | | | | | | | | | | | | | >> Recommended temperatures for heat processing | | | | | | | | | | | | | | Soft annealing: | Temperature [oC] | Cooling | | | | 780-820 | Furnace | | | | Annealing after decreasing stress: | Temperature [oC] | Cooling | | | | 600-650 | Furnace | | | | Hardening and tempering: | Austenization [oC] | Hardening | | | | 1000-1050 | Oil, pressure gas (N2), air, warm bath | | | | | | | |
|
|
Last Updated ( Salı, 30 Aralık 2008 )
|