STABIL (W.Nr. 1.2510), 100MnCrW4 | Chemical composition (%) | C | Mn | Si | P | S | Cr | Mo | Ni | 0.90-1.05 | 1.00-1.20 | 0.15-0.35 | max. 0.035 | max. 0.035 | 0.50-0.70 | 0.05-015 | 0.50-0.70 | | | | | | | | | | | | >> Standard | SEL 10. version (EN ISO 4957-95MnCr5-1.2825) | | | | | | | | | | | | Steel characteristics: | Medium alloyed steel for cold work, easy to temper. The steel is recognized for fine wear resistance, dimensional stability against wear and heat processing. | | Application: | Cutting and pressing devices, perforation and punching tool for sheet metal up to 6mm. Devices for cutting threads, measuring devices. | | Delivery condition: | Soft annealed steel, max.229 HB. | | Physical features: | Temperature [oC] | 20-100 | 20-200 | 20-300 | 20-400 | | Thermal expansion [10-6.K-1] | 12 | 12,6 | 13,1 | 13,1 | | Temperature [oC] | 20 | 350 | | | | Heat conductivity [W.m-1.K-1] | 33,4 | 32,1 | | | | | | | | | | | | | | | >> Recommended temperatures for heat processing | | | | | | | | | | | | | | Soft annealing: | Temperature [oC] | Cooling | | | | 740-770 | Furnace | | | | Annealing after decreasing stress: | Temperature [oC] | Cooling | | | | 600-650 | Furnace | | | | Hardening and tempering: | Austenization [oC] | Hardening | | | | 790-820 | Oil, warm bath | | | |
|
|
Last Updated ( Salı, 29 Eylül 2009 )
|