MAX SP MO5S (W.Nr. 1.3343), HS6-5-2C | Chemical composition (%) | C | Mn | Si | P | S | Cr | W | Mo | V | 1.45-1.6 | 0.2-0.6 | 0.1-0.6 | max.0.03 | max.0.03 | 11.0-13.0 | 0.7-1 | 0.7-1.01 | 0.7-1.02 | | | | | | | | | | | | >> Standard | EN ISO 4957 | | | | | | | | | | | | | | | | | | | Steel characteristics: | Fast cutting steel with high heat resistance, fine robustness, high compression strength, and fine wear resistance. The steel is a suitable material for hot chemical processing (CVD,PVD). | | | Application: | Common devices for machining and cutting, such as drills, millers, die stocks, broaches, devices for working with wood. Devices for forming and extruding metals under cold conditions. | | | Delivery condition: | Condition: Soft annealed steel, max.269 HB. | | | Physical features: | Temperature [oC] | 20-100 | 20-200 | 20-300 | 20-400 | | | Thermal expansion [10-6.K-1] | 10,8 | 11,8 | 12 | 12,5 | | | Temperature [oC] | 20 | 350 | 700 | | | | Heat conductivity [W.m-1.K-1] | 27,6 | 27,2 | 26,1 | | | | | | | | | | | | | | | | >> Recommended temperatures for heat processing | | | | | | | | | | | | | | | | Soft annealing: | Temperature [oC] | Cooling | | | | | 780-860 | Furnace | | | | | Annealing after decreasing stress: | Temperature [oC] | Cooling | | | | | 600-650 | Furnace | | | | | Hardening and tempering: | Austenization [oC] | Hardening | | | | | 1180-1230 | Oil, pressure gas (N2) air, warm bath | | | | | | | | | |
|
|
Last Updated ( Salı, 30 Aralık 2008 )
|